18.68.222 - Standard No. 24-42, pointing of unreinforced masonry walls.
The old or deteriorated mortar should be cut out, by means of a toothing chisel or nonimpact power tool to a uniform depth of three-fourths-inch, or until sound mortar is reached. Care must be taken not to damage the brick edges. After cutting is completed, remove all loose material with a brush, air, or water stream. Mortar mix shall be type "N" or "S" proportions as called for in the construction specifications, preferably as close to the original mortar proportion as possible. Prehydrate pointing mortar to reduce excessive shrinkage. To prehydrate mortar, thoroughly mix all ingredients dry, then mix again, adding only enough water to produce a damp unworkable mix which will retain its form when pressed into a ball. After keeping mortar in this dampened condition for one (1) to one and one-half (1½) hours, add sufficient water to bring it to the proper consistency that is somewhat drier than conventional masonry mortar. To ensure good bond, wet the mortar joints thoroughly before applying pointing mortar. The joints should not be visibly wet with free-standing water which must be absorbed into the wall. Pack mortar tightly in thin layers (one-fourth inch maximum) until the joint is filled, then tool to a smooth surface to match original profile.
(ORD-25-0019 § 1(Exh. A), 2025; ORD-22-0033 § 1(Exh. A), 2022; ORD-19-0031 § 1(Exh. A), 2019; ORD-16-0026 § 1(Exh. A), 2016)
Ask a question about Long Beach law
Corpus searches the Long Beach sections it holds and shows the ones that match, with their citations. Free, no sign-in.